Introduction of superalloy
Jul 16, 2018

definition

High-temperature alloy refers to a sort of metal material that is predicated on iron, nickel and metallic element and might work for a protracted time below the warm temperature of 600 °C and bound stress; and has high warm temperature strength, smart chemical reaction resistance and corrosion resistance. smart comprehensive properties reminiscent of fatigue performance and fracture toughness. The superalloy may be a single primary solid solution structure with smart structural stability and responsibleness at varied temperatures.

Based on the higher than performance characteristics, and high-alloy alloys have a high degree of alloying, conjointly referred to as "superalloy", it's a very important material wide employed in aviation, aerospace, petroleum, chemical, and construction. per the matrix component, the high-temperature alloy is additional divided into a high-temperature alloy reminiscent of associate degree iron base, a nickel base or a metallic element base. Iron-based superalloys usually use temperatures of solely 750 to 780 ° C. For heat-resistant components used at higher temperatures, nickel-based and refractory metal-based alloys square measure used. Nickel-based superalloys play a very necessary role within the entire superalloy business. they're wide employed in the manufacture of region jet engines and also the hottest finish components of assorted industrial gas turbines.


Quick Navigation
  • About Us
  • Product
  • News
  • Knowledge
  • Contact Us
  • Feedback
  • Newsletter
    Enter in your email address to receive deals and coupons.
    +86-18006107688
    +86-511-86456007 info@hltegang.com