Production process of nickel-based superalloy
Sep 19, 2018

Nickel-based alloys, particularly precipitation-strengthened alloys, contain high alloying components adore aluminium and metal. it's typically smelted during a vacuum induction chamber and remelted by a vacuum expendable chamber or an electrical dross chamber. the new operating adopts the shaping and rolling method. For the high alloying alloy, thanks to the poor thermoplasticity, it's rolled by extrusion or directly extruded by soft-cast steel (or unblemished steel). Casting alloys ar typically smelted during a vacuum induction chamber and created into components by vacuum remelting-precision casting.

Deformed alloys and partly solid alloys ar subjected to heat treatment, together with answer treatment, intermediate treatment and aging treatment. Taking Udmet five hundred alloy as associate degree example, its heat treatment system is split into four sections: answer treatment, 1175 ° C, 2 hours, air cooling; Treatment, 1080 ° C, 4 hours, air cooling; one aging treatment, 843 ° C, 24 hours, air cooling; secondary aging treatment, 760 ° C, 16 hours, air cooling. Get the desired tissue standing and sensible overall performance.


Quick Navigation
  • About Us
  • Product
  • News
  • Knowledge
  • Contact Us
  • Feedback
  • Newsletter
    Enter in your email address to receive deals and coupons.
    +86-18006107688
    +86-511-86456007 info@hltegang.com